Seedlabs
Source research

Biodegradation of Dental Resin-Based Composite—A Potential Factor Affecting the Bonding Effect: A Narrative Review

Xinwei Guo, Yiyan Yu, Shang Gao, Zhimin Zhang, Hongyan Zhao · 2022 · 75 citationsRead the paper

In recent years, although resin composite has played an important role in the restoration of tooth defects, it still has several disadvantages, including being biodegraded by saliva, bacteria and other enzymes in the oral cavity, which may result in repair failure. This factor is not conducive to the long-term survival of the prosthesis in the mouth. In this article, we review the causes, influencing factors and prevention methods of resin biodegradation. Biodegradation is mainly caused by esterase in saliva and bacteria, which breaks the ester bond in resin and causes the release of monomers. The mechanical properties of the prosthesis can then be affected. Meanwhile, cathepsin and MMPs are activated on the bonding surface, which may decompose the dentin collagen. In addition, neutrophils and residual water on the bonding surface can also aggravate biodegradation. Currently, the primary methods to prevent biodegradation involve adding antibacterial agents to resin, inhibiting the activity of MMPs and enhancing the crosslinking of collagen fibers. All of the above indicates that in the preparation and adhesion of resin materials, attention should be paid to the influence of biodegradation to improve the prosthesis's service life in the complex environment of the oral cavity.

What the full text shows

Shown in the lab
  • S. mutans esterase SMU-118c almost completely hydrolyzes Bis-GMA within 125 hours. — ~100% hydrolysis vs. 11.9-17.6% for TEGDMA (125 hours incubation)
  • Incubation of Bis-GMA-based resin with cholesterol esterase (CE) leads to microleakages at the bonding interface. — Observed on day 30 (In vitro buffer containing CE)
  • Aging in artificial saliva and esterase causes a dramatic decline in radial tensile strength, elasticity, and fracture toughness. — '' (180 days aging)
  • S. mutans co-culture increases resin surface roughness and releases Bis-HPPP. — Bis-HPPP detected after 14 days (Co-culture with Bis-GMA-based resin)
  • Polyurethane-modified Bis-GMA exhibits higher stability and resistance to hydrolysis compared to standard Bis-GMA. — '' (Exposure to human saliva)
  • Enterococcus faecalis degrades dentin collagen on the bonding interface. — Degradation observed after 24 hours (Incubation within demineralized dentin)
Setup
Review of in vitro and in vivo studies involving Bis-GMA, TEGDMA, and UDMA resins, and bacteria including S. mutans and E. faecalis.
How
Narrative review of existing literature analyzing the effects of salivary enzymes, bacterial esterases, and proteases on dental resin composites and dentin.
Limitations
Lack of quantitative data for UDMA biodegradation · Review nature means results are aggregated from multiple different study protocols

Summarized by Gemma 4 from the open-access full text · 16 Nov 2026. Read it