The Mechanical Properties of Orthodontic Aligners of Clear Aligner After Intraoral Use in Different Time Periods
Kalliopi Siotou, Theofanis D. Chountalas, Athanasios Katsavrias, Charalampos Siotos, Konstantinos Mpalias, Dionisis Semitekolos et al. · 2024 · 16 citationsRead the paper
OBJECTIVE: Although the technique of orthodontic aligners has risen in popularity, their mechanical properties have not been thoroughly investigated. The aim of this study was to evaluate the mechanical properties of the orthodontic aligners Clear Aligner after intraoral use for 7, 10 and 14 days, and to compare them with as-received aligners (0 days). It was also sought to examine the properties of the unprocessed raw material (polyethylene glycol terephthalate) used to manufacture these aligners. MATERIALS/METHODS: Thirty-two aligners by four patients were evaluated and studied at 0, 7, 10, 14 days of use. Each aligner was divided into three segments (two posterior and one anterior), which resulted in 96 samples. Also, 16 samples of unprocessed material were studied. For all samples, elastic modulus, ultimate tensile stress (UTS) and yield stress were calculated by conducting tensile testing. Additionally, material hardness was tested. The two-tailed Mann-Whitney test was performed, having set the level of significance at p = 0.05. RESULTS: Analysis of the measurements indicated a statistically significant decrease in elastic modulus between days 0 and 14 of use, of UTS between days 0 and 7, 7 and 10, and of yield stress between days 0 and 7. For hardness, in every period, posterior segments demonstrated significantly higher values than anterior segments. All properties of the unprocessed material were statistically significantly higher than the processed samples. CONCLUSIONS: The unprocessed material presented significant differences in every property tested in comparison to the processed aligners. The processed material showed further deterioration over time during use. The present study provides evidence that thermoforming and ageing affect the mechanical properties of the aligners.
What the full text shows
Tested in real conditions- Elastic modulus significantly decreased after 14 days of intraoral use. — 911.66 ± 139.90 MPa (day 0) to 746.41 ± 145.41 MPa (day 14) (Processed aligners)
- Ultimate Tensile Stress (UTS) significantly decreased between day 0 and day 7, and between day 7 and day 10. — 35.12 ± 3.83 MPa (day 0) to 30.85 ± 6.46 MPa (day 7) to 23.43 ± 11.64 MPa (day 10) (Processed aligners)
- Yield stress significantly decreased after 7 days of intraoral use. — 33.05 ± 3.76 MPa (day 0) to 28.90 ± 6.07 MPa (day 7) (Processed aligners)
- Posterior segments maintained significantly higher elastic modulus than anterior segments after 14 days of use. — 814.68 ± 118.64 MPa (posterior) vs 609.87 ± 85.79 MPa (anterior) (Day 14 of intraoral use)
- Unprocessed PETG material exhibited significantly higher mechanical properties than thermoformed aligners. — Elastic modulus: 1186.82-1269.53 MPa; UTS: 51.76-51.89 MPa; Yield stress: 49.44-50.87 MPa (Comparison of raw PETG vs day 0 aligners)
- Posterior segments showed significantly higher Shore D hardness than anterior segments across all time periods. — p < 0.01 (Intraoral use 0-14 days)
- Setup
- 96 samples from 32 aligners (4 patients) divided into anterior and posterior segments, plus 16 unprocessed PETG samples.
- How
- Tensile testing (ISO 14577-2016) was used to measure elastic modulus, UTS, and yield stress, while a Shore D durometer (ASTM D2240) measured hardness. Samples were taken from unprocessed PETG, as-received aligners, and aligners used intraorally for 7, 10, and 14 days.
- Limitations
- Small patient sample size (n=4) · 16.96% of samples excluded due to microcracks/flaws during preparation · Short observation window (max 14 days)
Summarized by Gemma 4 from the open-access full text · 16 Nov 2026. Read it